耦合孪生的TWIP钢单晶体塑性变形行为模拟研究
|
|
孙朝阳, 郭祥如, 黄杰, 郭宁, 王善伟, 杨竞
|
MODELLING OF PLASTIC DEFORMATION ON COUPLING TWINNING OF SINGLE CRYSTAL TWIP STEEL
|
|
SUN Chaoyang, GUO Xiangru, HUANG Jie, GUO Ning, WANG Shanwei, YANG Jing
|
|
| 表1 孪生诱导塑性(TWIP)钢12个滑移系的滑移面和滑移方向 |
| Table 1 Slip planes and slip directions for twinning induced plasticity (TWIP) steel with 12 slip systems |
|
| Slip system | Slip plane | Slip direction | Slip system | Slip plane | Slip direction | | a1 | | | b1 | | | | a2 | | | b2 | | | | a3 | | | b3 | | | | c1 | | | d1 | | | | c2 | | | d2 | | | | c3 | | | d3 | | |
|
|
|