核级低合金钢高温水腐蚀疲劳机制及环境疲劳设计模型
|
|
吴欣强, 谭季波, 徐松, 韩恩厚, 柯伟
|
CORROSION FATIGUE MECHANISM OF NUCLEAR-GRADE LOW ALLOY STEEL IN HIGH TEMPERATURE PRESSURIZED WATER AND ITS ENVIRONMENTAL FATIGUE DESIGN MODEL
|
|
WU Xinqiang, TAN Jibo, XU Song, HAN En-Hou, KE Wei
|
|
| 表3 某压水堆进水管嘴的疲劳延寿评估[31] |
| Table 3 Life extension of a pressurized water reactor inlet nozzle[31] |
|
| Load pair | Salt | Nenv | 40 a | | 60 a | | N40 | U40 | | N60 | U60 | | Cooldown/plant load | 416.6 | 1458 | 90 | 0.062 | | 135 | 0.093 | | Leak test/plant unload | 330.8 | 1534 | 200 | 0.130 | | 300 | 0.196 | | Heatup/plant load | 270.4 | 4263 | 90 | 0.021 | | 135 | 0.032 | | Plant load/unload | 143.6 | 58406 | 14620 | 0.250 | | 21930 | 0.375 | | Plant unload/upset | 136.6 | 73899 | 480 | 0.007 | | 720 | 0.010 | | Plant undload/OBE | 98.7 | 265677 | 200 | 0.001 | | 300 | 0.001 | | Plant unload/step load | 87.6 | 729360 | 520 | 0.001 | | 780 | 0.001 | | | | | Total 0.472 | | | Total 0.708 |
|
|
|