Nb含量对NiCrFe-7焊缝金属组织、缺陷和力学性能的影响*
|
|
莫文林, 张旭, 陆善平, 李殿中, 李依依
|
EFFECT OF Nb CONTENT ON MICROSTRUCTURE, WELDING DEFECTS AND MECHANICAL PROPERTIES OF NiCrFe-7 WELD METAL
|
|
MO Wenlin, ZHANG Xu, LU Shanping, LI Dianzhong, LI Yiyi
|
|
| 表1 焊丝合金成分的设计 |
| Table 1 Composition design of filler wires |
|
| Sample | Nb | Al | Ti | C | Si | Fe | Cr | Ni | | 0Nb | <0.02 | 0.1~0.2 | 0.2~0.4 | 0.02~0.04 | 0.1~0.3 | 9~11.5 | 29.5~30.5 | Bal. | | 0.4Nb | 0.30~0.50 | 0.1~0.2 | 0.2~0.4 | 0.02~0.04 | 0.1~0.3 | 9~11.5 | 29.5~30.5 | Bal. | | 0.7Nb | 0.60~0.80 | 0.1~0.2 | 0.2~0.4 | 0.02~0.04 | 0.1~0.3 | 9~11.5 | 29.5~30.5 | Bal. | | 0.85Nb | 0.80~0.95 | 0.1~0.2 | 0.2~0.4 | 0.02~0.04 | 0.1~0.3 | 9~11.5 | 29.5~30.5 | Bal. | | 1.1Nb | 1.00~1.20 | 0.1~0.2 | 0.2~0.4 | 0.02~0.04 | 0.1~0.3 | 9~11.5 | 29.5~30.5 | Bal. |
|
|
|