模拟工业-海岸大气中pH值对Q235B钢腐蚀行为的影响*
|
|
陈文娟, 郝龙, 董俊华, 柯伟, 文怀梁
|
EFFECT OF pH VALUE ON THE CORROSION EVOLUTION OF Q235B STEEL IN SIMULATED COASTAL-INDUSTRIAL ATMOSPHERES
|
|
CHEN Wenjuan, HAO Long, DONG Junhua, KE Wei, WEN Huailiang
|
|
| 表2 Q235B钢在模拟工业-海岸大气中9条腐蚀增重曲线的分段拟合结果 |
| Table 2 Fitting results of corrosion mass gain of Q235B steel in the nine simulated coastal-industrial atmospheres in Table 1 (y is lgDW, x is lgN, lgA is the constant and n is the slop in the Eq.(3), R2 is the fitting correlation coefficient) |
|
| Atmosphere | 1st stage | 2nd stage | 3rd stage | 4th stage | | No.1 | y=-0.108+0.991x | - | - | - | | R2=0.998 | | | | | No.2 | y=-0.069+0.958x | - | - | - | | R2=0.998 | | | | | No.3 | y=-0.122+0.996x | - | - | - | | R2=0.999 | | | | | No.4 | y=-0.094+1.039x | - | - | - | | R2=0.999 | | | | | No.5 | y=-0.044+1.006x | - | - | - | | R2=0.999 | | | | | No.6 | y=-0.072+1.031x | - | - | - | | R2=0.999 | | | | | No.7 | y=0.057+0.772x | y=0.232+0.566x | y=-0.725+1.401x | y=-0.176+0.994x | | R2=0.977 | R2=0.992 | R2=0.996 | R2=0.999 | | No.8 | y=0.062+0.849x | y=0.256+0.605x | y=-0.664+1.405x | y=-0.096+1.007x | | R2=0.997 | R2=0.992 | R2=0.996 | R2=0.995 | | No.9 | y=0.047+0.795x | y=0.199+0.614x | y=-0.705+1.398x | y=-0.014+0.877x | | R2=0.981 | R2=0.964 | R2=0.995 | R2=0.998 |
|
|
|