| 表2 不同方法的性能对比分析 |
| Table 2 Performance analysis of different methods |
|
Sample No. | / mm | / % | / mm | / % | / mm | / % | | 1 | 81.5±5.7 | 12.57 | 72.9±2.9 | 0.69 | 72.7±1.9 | 0.41 | | 2 | 83.6±8.5 | 1.33 | 81.2±3.5 | -1.58 | 82.3±2.8 | -0.24 | | 3 | 85.5±10.6 | -5.63 | 95.9±4.1 | 5.85 | 91.7±4.0 | 1.21 | | 4 | 98.2±8.3 | -7.01 | 102.0±4.5 | -3.41 | 104.2±4.4 | -1.33 | | 5 | 135.7±9.0 | 0.22 | 131.5±5.7 | -2.88 | 134.3±2.7 | -0.81 | | 6 | 143.9±10.1 | 1.41 | 145.0±6.5 | 2.18 | 143.3±3.5 | 0.99 |
|
|
|