TC4钛合金搅拌摩擦焊厚度方向的显微组织*
|
姬书得 1( ),温泉 1,马琳 1,李继忠 2,张利 1
|
MICROSTRUCTURE ALONG THICKNESS DIRECTION OF FRICTION STIR WELDED TC4 TITANIUM ALLOY JOINT
|
Shude JI 1( ),Quan WEN 1,Lin MA 1,Jizhong LI 2,Li ZHANG 1
|
|
图6. 转速为300和350 r/min时TC4钛合金搅拌摩擦焊测温点的模拟与NiCr-NiSi热电偶测温实验热循环曲线
|
Fig.6. Simulated and NiCr-NiSi thermocouple temperature measurement of experimental thermal cycle curves of measurement poins during friction stir welding (FSW) for TC4 titanium alloy at rotational speed of 300 and 350 r/min (l—distance from weld center) |
|
|
|
|