图3. 扫描速率为1.667 mV/s 时KSCN浓度对409L钢在30 ℃的0.5%H2SO4溶液中DL-EPR测试结果的影响

Fig.3. Effects of KSCN concentration (c) on DL-EPR test for 409L steel in 0.5%H2SO4 solution with scanning rate 1.667 mV/s at 30 ℃ (Ra—intergranular corrosion sensitivity)