镍基单晶高温合金冷热循环过程中圆孔周围裂纹萌生与扩展行为
王莉1(),周忠娇1,张少华1sup,降向冬2,楼琅洪1,张健1
CRACK INITIATION AND PROPAGATION AROUND HOLES OF Ni-BASED SINGLE CRYSTAL SUPERALLOY DURING THERMAL FATIGUE CYCLE
Li WANG1(),Zhongjiao ZHOU1,Shaohua ZHANG1,Xiangdong JIANG2,Langhong LOU1,Jian ZHANG1

图2. 镍基单晶高温合金完全热处理后的OM像和γ’形貌

Fig.2. OM image (a) and γ’ morphology (b) of Ni-based single crystal superalloy after full heat treatment