Hf对第二代镍基单晶高温合金DD11高温低应力持久性能的影响
赵云松1,2,张剑2,骆宇时2,唐定中2,冯强1,3()
EFFECTS OF Hf ON HIGH TEMPERATURE LOW STRESS RUPTURE PROPERTIES OF A SECOND GENERATION Ni-BASED SINGLE CRYSTAL SUPERALLOY DD11
Yunsong ZHAO1,2,Jian ZHANG2,Yushi LUO2,Dingzhong TANG2,Qiang FENG1,3()

图10. 合金在1100 ℃, 140 MPa持久断裂后γ/γ’界面位错网络

Fig.10. γ/γ’ interfacial dislocation networks in alloys Hf-1 (a), Hf-2 (b), Hf-3 (c) and Hf-4 (d) after stress-rupture under 1100 ℃ and 140 MPa