高温合金铸锭均匀化程度对开坯热变形的再结晶影响
|
|
EFFECT OF EXTENT OF HOMOGENIZATION ON THE HOT DEFORMATION RECRYSTALLIZATION OF SUPERALLOY INGOT IN COGGING PROCESS
|
|
图16. 含枝晶的GH4738合金铸态组织热变形中的再结晶位置 |
Fig.16. Recrystallization positions of as-cast GH4738 alloy after hot compression in small deformation zone (a) and large deformation zone (b) (A, B, C show recrystallization site near carbide particles) |
![]() |