高温合金铸锭均匀化程度对开坯热变形的再结晶影响
|
|
EFFECT OF EXTENT OF HOMOGENIZATION ON THE HOT DEFORMATION RECRYSTALLIZATION OF SUPERALLOY INGOT IN COGGING PROCESS
|
|
图14. 不同均匀化程度GH4738合金试样在1150 ℃下以0.1 s-1变形量30%热变形的真应力-真应变曲线 |
Fig.14. True stress-true strain curves of hot compressed (1150 ℃, 0.1 s-1, 30%) GH4738 alloy under different homogenizations |
![]() |