高温合金铸锭均匀化程度对开坯热变形的再结晶影响
|
|
EFFECT OF EXTENT OF HOMOGENIZATION ON THE HOT DEFORMATION RECRYSTALLIZATION OF SUPERALLOY INGOT IN COGGING PROCESS
|
|
图10. GH3625合金铸态、保温态和变形态的显微组织 |
Fig.10. Microstructures of as-cast GH3625 alloy (a), and soaking at 1250 ℃ for 5 min (b), hot compressed at 1100 ℃, 0.01 s-1, 50% (c) |
![]() |