高温合金铸锭均匀化程度对开坯热变形的再结晶影响
|
|
EFFECT OF EXTENT OF HOMOGENIZATION ON THE HOT DEFORMATION RECRYSTALLIZATION OF SUPERALLOY INGOT IN COGGING PROCESS
|
|
图2. 690合金均匀化过程中残余偏析指数和晶粒尺寸的变化 |
Fig.2. Changes of segregation index and grain size with time of 690 alloy during homogenization treatment |
![]() |