GH3535合金在FLiNaK熔盐中的腐蚀行为
刘涛1,2,董加胜2(),谢光2,王义胜3,李辉2,李志军4,周兴泰4,楼琅洪2
CORROSION BEHAVIOR OF GH3535 SUPERALLOY IN FLiNaK MOLTEN SALT
Tao LIU1,2,Jiasheng DONG2(),Guang XIE2,Yisheng WANG3,Hui LI2,Zhijun LI4,Xingtai ZHOU4,Langhong LOU2

图7. 无Al2O3涂层GH3535合金在FLiNaK熔盐中腐蚀反应示意图

Fig.7. Corrosion schematic of the corrosion reaction of the GH3535 specimen without Al2O3 film during long term thermal exposure in FLiNaK molten salt at 700 ℃ for 400 h