SiCf/TC17复合材料拉伸行为研究
|
STUDY ON TENSILE BEHAVIOR OF SiCf/TC17 COMPOSITES
|
图7. SiCf/TC17复合材料室温拉伸断口中起伏较大区域的纵剖面典型形貌 |
Fig.7. Typical morphologies of longitudinal section related to the irregular fracture region in fracture surface of the SiCf/TC17 composites at room temperature (a) partial macromorphology of longitudinal section (b) multiple fracture of tungsten core and matrix plastic deformation near the damaged fiber (c) multiple fracture of reaction layer near damaged fiber (d) irregular fracture surface and micro-cavities of matrix |
![]() |