SiCf/TC17复合材料拉伸行为研究
|
STUDY ON TENSILE BEHAVIOR OF SiCf/TC17 COMPOSITES
|
图5. SiCf/TC17复合材料773 K拉伸断口形貌 |
Fig.5. Fracture morphologies of the fracture surface of the SiCf/TC17 composites at 773 K (a) panorama of fracture surface (b) dimples in the TC17 canning (c) local irregular fracture surface (d) tunsgen "pull-out" (e) longitudinal matrix cracks (f) interface debonding and matrix damage in a ductile way |
![]() |