电参数对AZ31B镁合金微弧氧化膜微观形貌及耐蚀性的影响
崔学军, 王荣, 魏劲松, 白成波, 林修洲

Effect of Electrical Parameters on Micromorphology and Corrosion Resistance of Micro-arc Oxidation Coating on AZ31B Mg Alloy
CUI Xuejun, WANG Rong, WEI Jinsong, BAI Chengbo, LIN Xiuzhou
表3 与图9极化曲线相对应的拟合电参数值
Duty cycle -Ecorr / mV icorr / μAcm-2 Rp / kΩcm2
15% 1514 1.1110 18.045
30% 1474 0.3194 114.902
45% 1530 0.3365 26.552
60% 1419 0.5898 12.462
75% 1506 0.9311 6.062