Organic-inorganic hybrid system | Functional additive agent | Substrate | Reference | GPTMS, TEOS | | Copper | [32] | GPTMS, TMOS | 2-methyl piperidine | AZ91D Mg-alloy | [33] | BTES | | AA1050 Al-alloy | [34] | TAP, TPOZ, GPTMS | TMSP | AZ31B Mg-alloy | [35] | TEOS, GMA, MAPTS, EGDMA | Ce(NO3)3·6H2O | AA2024T3 Al-alloy | [36] | GPTMS, TIP | Ce(NO3)3, 8-hydroxyquinoline | ZK30 Mg-alloy | [37] | BTESPT | | AZ31 Mg-alloy | [38] | MTEOS | Mg(NO3)2 | AA2024-T3 Al-alloy | [39] | BTSE | | Cold rolled Al-sheets | [40] | BTESPT | | WE54 Mg-alloy | [41] | GPTMS, TEOS | Zn(NO3)2 | AZ91D Mg-alloy | [42] | GPTMS, TEOS | | AZ91D Mg-alloy | [43] | TMOS, DEDMS, ZTB | Ce(NO3)3·6H2O | AZ91 Mg-alloy | [44] | GPTMS, TPOZ | | AA2024T3 Al-alloy | [45] | TEOS | Polyaniline | AZ31 Mg-alloy | [46] | BTSE | | ZE41 Mg-alloy | [47] | MPTMS | | Copper plates | [48] | Zr(OC4H9)4, ZrO(NO3)2 | 2-mercaptobenzothiazole, Ce(NO3)3 | AA2024-T3 Al-alloy | [49] | MPTMS | | Die-cast AZ91 Mg-alloy | [50] | TES, TEOS | Zirconium and cerium oxide nanoparticles | AA-2024-T3 Al-alloy | [51] | MTES | Ce(NO3)3 | AZ91 Mg-alloy | [52] | GPTMS, TPOZ | Thermally activated hydrotalcite | AA2024-T3 Al-alloy | [53] | Ce(NO3)3 | | AA2024,AA3105 Al-alloy and AZ-91, AZ-31 Mg-alloy | [54] | GPTMS | POSS | AA2024 Al-alloy | [55] | GPTMS, TEOS, MTES, BPA | Ce2(SO4)3 | AA2024 Al-alloy | [56] | GPTMS, TPOZ | Dried and Calcined Red mud particles | AA2024-T3 Al-alloy | [57] |
|