表1 Cr在不同熔盐体系中的平衡溶解浓度[3] |
Table 1 Equilibrium level of Cr dissolved in various salts[3] |
|
Salt mixture | ZrF4 or BeF2 mol.% | [UF4] mol.% | [Cr] at 600 ℃ 10-6 mol | [Cr] at 800 ℃ 10-6 mol | FLiNaK | 0 | 2.5 | 1100 | 2700 | LiF-ZrF4 | 48 | 4.0 | 2900 | 3900 | NaF-ZrF4 | 50 | 4.1 | 2300 | 2550 | NaF-ZrF4 | 47 | 4.0 | 1700 | 2100 | NaF-ZrF4 | 41 | 3.7 | 975 | 1050 | KF-ZrF4 | 48 | 3.9 | 1080 | 1160 | NaF-LiF-ZrF4 (22-22-23) | 23 | 2.5 | 550 | 750 | LiF-BeF2 | 48 | 1.5 | 1470 | 2260 |
|
|
|