腐蚀微生物硫酸盐还原菌在不同荷电状态表面的初始附着行为
|
Initial Adhesion of Sulfate Reducing Bacteria on Materials with Different Surface Charge
|
图2. 3种SAMs表面在含有5 mmol/L [Fe(CN)6]3-/4-的PBS中的电化学阻抗谱 |
Fig.2. Nyquist diagrams for the Faradaic impedance measurement of three kinds of SAMs in 0.2 mol/L PBS solution (pH 7.4) containing 5 mmol/L [Fe(CN)6]3-/[Fe(CN)6]4-(1∶1): (a) AH-Au and MH-Au, (b) MHA-Au |
![]() |