镍基合金800H的腐蚀性能研究
沈朝,吴恋恋,张乐福,段振刚,孙耀
Corrosion Behavior of Nickel Base Alloy 800H in High-temperature and High-pressured Water
Zhao SHEN,Lianlian WU,Lefu ZHANG,Zhengang DUAN,Yao SUN

图3.

Fig.3.

800H在空气中的机械强度和屈服强度随温度的变化速率曲线及抗拉强度随温度的变化速率曲线