| Heat conductivity of graphite crucible, lgraphite | 131.06-0.0425T | W/(m·K) |
| Density of graphite crucible, rgraphite | 2200 | kg/m3 |
| Specific heat of graphite crucible, Cpgraphite | 0.71 | kJ/(kg·K) |
| Emissivity of heater, eheater | 0.98[23] | |
| Emissivity of graphite crucible, ecrucible | 0.98[23] | |
| Emissivity of copper and chiller, ecopper | 0.78[23] | |
| Convection heat transfer coefficient, hcrucible/gas | 200* | W/(m2·K) |
| Convection heat transfer coefficient, hmelt/gas | 200* | W/(m2·K) |
| Convection heat transfer coefficient, hchiller/gas | 200* | W/(m2·K) |
| Interfacial heat transfer coefficient, hcrucible/solid copper | 3000[24] | W/(m2·K) |
| Interfacial heat transfer coefficient, hcrucible/copper melt | 5000* | W/(m2·K) |
| Interfacial heat transfer coefficient, hchiller/crucible | 3000[24] | W/(m2·K) |
| Interfacial heat transfer coefficient, hchiller/water | 8000[25] | W/(m2·K) |