一种细晶铸造镍基高温合金的组织与力学性能* |
|||||||||||||||
| 杨金侠, 孙元, 金涛, 孙晓峰, 胡壮麒 | |||||||||||||||
|
MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A Ni-BASED SUPERALLOY WITH REFINED GRAINS |
|||||||||||||||
| YANG Jinxia, SUN Yuan, JIN Tao, SUN Xiaofeng, HU Zhuangqi | |||||||||||||||
| 表2 在760 ℃和应力662 MPa时合金在不同条件的持久性能 | |||||||||||||||
| Table 2 Stress-rupture properties of tested alloy at 760 ℃ and 662 MPa in different conditions | |||||||||||||||
|
|||||||||||||||