2099合金热变形过程中的动态软化机制*
|
|
张飞, 沈健, 闫晓东, 孙建林, 蒋呐, 周华
|
DYNAMIC SOFTENING MECHANISM OF 2099 ALLOY DURING HOT DEFORMATION PROCESS
|
|
ZHANG Fei, SHEN Jian, YAN Xiaodong, SUN Jianlin, JIANG Na, ZHOU Hua
|
|
| 表1 2099合金的热激活参数 |
| Table 1 Thermal activation parameters of 2099 alloy |
|
T / ℃ | Q / (K·mol-1) | V / (10-30 m3) and lnZ parameter | | 0.001 s-1 | 0.01 s-1 | 0.1 s-1 | 1 s-1 | 10 s-1 | | 300 | 147.8 | 57.7 / 35.5 | 83.3 / 37.8 | 79.9 / 40.1 | 38.0 / 42.4 | 20.5 / 44.7 | | 340 | 163.6 | 91.0 / 32.8 | 93.0 / 35.1 | 86.4 / 37.7 | 74.2 / 39.7 | 60.9 / 41.9 | | 380 | 178.2 | 196.0 / 30.3 | 134.6 / 32.6 | 106.1 / 34.9 | 87.5 / 37.5 | 76.4 / 39.5 | | 420 | 188.9 | 245.3 / 28.2 | 162.2 / 30.5 | 127.6 / 32.8 | 108.7 / 35.1 | 99.7 / 37.4 | | 460 | 208.7 | 374.8 / 26.3 | 194.6 / 28.6 | 136.8 / 30.9 | 133.2 / 33.2 | 171.5 / 35.5 | | 500 | 188.7 | 444.7 / 24.5 | 260.3 / 26.8 | 197.6 / 29.2 | 187.2 / 31.5 | 222.3 / 33.8 |
|
|
|