20SiMn钢在恒定pH值的碳酸盐溶液中的腐蚀行为*
|
|
曹凤婷, 魏洁, 董俊华, 柯伟
|
CORROSION BEHAVIOR OF 20SiMn STEEL REBAR IN CARBONATE/BICARBONATE SOLUTIONS WITH THE SAME pH VALUE
|
|
CAO Fengting, WEI Jie, DONG Junhua, KE Wei
|
|
| 表3 0.05 mol/L 碳酸盐缓冲液中的EIS 拟合结果 |
| Table 3 EIS fitting results of the parameters in 0.05 mol/L carbonate buffer solution |
|
Immerse time d | Rs Ω·cm2 | Q1 Ω-1·cm-2·sn | n1 | R1 Ω·cm2 | Qct Ω-1·cm-2·sn | nct | Rct Ω·cm2 | | 1 | 29.71 | 4.796×10-5 | 0.9682 | 1.004×106 | 1.034×10-4 | 0.8553 | 24940 | | 2 | 35.20 | 4.731×10-5 | 0.9819 | 1.145×106 | 8.242×10-5 | 0.8585 | 36300 | | 3 | 30.27 | 4.414×10-5 | 0.9718 | 1.256×106 | 8.412×10-5 | 0.8653 | 36490 | | 4 | 27.96 | 4.642×10-5 | 0.9641 | 1.078×106 | 8.349×10-5 | 0.8648 | 34270 | | 5 | 26.59 | 4.457×10-5 | 0.9794 | 1.196×106 | 7.351×10-5 | 0.8660 | 44470 | | 6 | 33.17 | 4.354×10-5 | 0.9792 | 1.236×106 | 7.237×10-5 | 0.8653 | 46890 | | 7 | 24.01 | 4.182×10-5 | 0.9758 | 1.254×106 | 7.383×10-5 | 0.8678 | 45270 |
|
|
|