20SiMn钢在恒定pH值的碳酸盐溶液中的腐蚀行为*
|
|
曹凤婷, 魏洁, 董俊华, 柯伟
|
CORROSION BEHAVIOR OF 20SiMn STEEL REBAR IN CARBONATE/BICARBONATE SOLUTIONS WITH THE SAME pH VALUE
|
|
CAO Fengting, WEI Jie, DONG Junhua, KE Wei
|
|
| 表2 0.01 mol/L 碳酸盐缓冲液中的EIS 拟合结果 |
| Table 2 EIS fitting results of the parameters in 0.01 mol/L carbonate buffer solution |
|
Immerse time d | Rs Ω·cm2 | Qct Ω-1·cm-2·sn | nct | Rct Ω·cm2 | W Ω-1·cm-2·s0.5 | | 1 | 28.65 | 8.905×10-4 | 0.7949 | 2348 | 0.00955 | | 2 | 59.61 | 0.001 | 0.7961 | 2027 | 0.00811 | | 3 | 68.75 | 9.561×10-4 | 0.7811 | 1776 | 0.01129 | | 4 | 58.43 | 9.039×10-4 | 0.7756 | 1965 | 0.00694 | | 5 | 75.14 | 9.633×10-4 | 0.7520 | 2186 | 0.00623 | | 6 | 56.39 | 9.285×10-4 | 0.7552 | 2280 | 0.00439 | | 7 | 64.84 | 8.534×10-4 | 0.7465 | 2371 | 0.00193 |
|
|
|