20SiMn钢在恒定pH值的碳酸盐溶液中的腐蚀行为*
|
|
曹凤婷, 魏洁, 董俊华, 柯伟
|
CORROSION BEHAVIOR OF 20SiMn STEEL REBAR IN CARBONATE/BICARBONATE SOLUTIONS WITH THE SAME pH VALUE
|
|
CAO Fengting, WEI Jie, DONG Junhua, KE Wei
|
|
| 表1 0.437×10-3 mol/L NaOH溶液中的EIS拟合结果 |
| Table 1 EIS fitting results of the parameters in 0.437×10-3 mol/L NaOH solution |
|
Immerse time d | Rs Ω·cm2 | Q1 Ω-1·cm-2·sn | n1 | R1 Ω·cm2 | Qdl Ω-1·cm-2·sn | nct | Rct Ω·cm2 | | 1 | 33.19 | 0.00103 | 0.8726 | 52.35 | 7.025×10-4 | 0.8473 | 1103 | | 2 | 42.55 | 0.00175 | 0.9408 | 36.88 | 7.125×10-4 | 0.8522 | 1454 | | 3 | 78.33 | 0.09831 | 1 | 263.3 | 7.515×10-4 | 0.827 | 1207 | | 4 | 90.28 | 0.00237 | 0.5975 | 1620 | 0.00415 | 1 | 312 | | 5 | 67.82 | 0.00187 | 0.6404 | 1057 | 0.0057 | 1 | 161 | | 6 | 70.91 | 0.00124 | 1 | 8.396 | 0.00154 | 0.7005 | 1186 | | 7 | 34.11 | 1.937×10-8 | 0.8873 | 106.2 | 0.00175 | 0.6847 | 1095 |
|
|
|