低温挤压Mg-4Zn-2Al-2Sn合金的组织与力学性能研究*
赵东清, 周吉学, 刘运腾, 董旭光, 王晶, 杨院生

MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Mg-4Zn-2Al-2Sn ALLOYS EXTRUDED AT LOW TEMPERATURES
ZHAO Dongqing, ZHOU Jixue, LIU Yunteng, DONG Xuguang, WANG Jing, YANG Yuansheng
表2 挤压Mg-4Zn-2Al-2Sn合金拉伸与压缩性能
Extrusion temperature
℃
Tensile property Compressive property
R

Yield strength
MPa
Ultimate strength
MPa
Elongation
%
Yield strength MPa Ultimate strength
MPa
Elongation
%
225 211.7 317.5 27.6 186.3 451.0 -17.6 0.88
250 176.7 296.3 24.0 158.6 442.0 -18.0 0.89
275 173.8 293.8 23.6 165.8 458.7 -16.5 0.95