表2 4种材料高速冲击力学参数 |
|
Material | Impact load / MPa | Strain rate / s-1 | Reduction of H / % | TRIP steel | 0.30 | 1.2×104 | 9.7 | | 0.50 | 1.7×104 | 21.6 | | 0.55 | 1.9×104 | 23.2 | | 0.60 | 2.0×104 | 35.0 | Pure Cu | 0.30 | 1.3×104 | 21.2 | | 0.55 | 1.9×104 | 40.0 | IF steel | 0.30 | 1.1×104 | 10.0 | | 0.55 | 1.7×104 | 26.4 | Armor steel | 0.20 | 0.3×104 | 0.7 | | 0.25 | 0.4×104 | 2.2 | | 0.30 | 0.45×104 | 4.0 |
|
|
|