DD6高温合金定向凝固枝晶生长的数值模拟研究*
|
|
张航, 许庆彦, 史振学, 柳百成
|
NUMERICAL SIMULATION OF DENDRITE GRAIN GROWTH OF DD6 SUPERALLOY DURING DIRECTIONAL SOLIDIFICATION PROCESS
|
|
ZHANG Hang, XU Qingyan, SHI Zhenxue, LIU Baicheng
|
|
| 表1 DD6合金的模拟用参数 |
| Table 1 Simulating parameters of DD6 superalloy |
|
| Parameter | Unit | Value | | Liquidus | K | 1672[42] | | Solidus | K | 1615[42] | | Thermal conductivity | kJ/(m·s·K) | 0.0332[42] | | Specific heat | kJ/(kg·K) | 0.773[42] | | Density | kg/m3 | 8780[42] | | Latent heat | kJ/kg | 99[42] | | Mass fraction | % | 39.006* | | Partition | | 0.788* | | Liquidus slope | ℃/% | -3.95* | | Diffusion coefficient in liquid (DL) | m2/s | 3.6×10-9 | | Diffusion coefficient in solid (DS) | m2/s | 1.0×10-12 | | Gibbs -Thomson coefficient (G) | k·m | 3.65×10-7[17] | | Anisotropy intensity coefficient (g) | | 0.04 |
|
|
|