氧化膜结构及内应力对新锆合金腐蚀机理的影响
|
|
章海霞, 李中奎, 周廉, 许并社, 王永祯
|
EFFECTS OF STRUCTURE AND INTERNAL STRESSES IN OXIDE FILMS ON CORROSION MECHANISM OF NEW ZIRCONIUM ALLOY
|
|
ZHANG Haixia, LI Zhongkui, ZHOU Lian, XU Bingshe, WANG Yongzhen
|
|
| 表1 NZ2合金在360 ℃含锂水和400 ℃蒸汽中腐蚀不同时间后的参数 |
| Table 1 Parameters of NZ2 alloy corroded in 360 ℃ lithiated water and 400 ℃ steam for different times |
|
| Condition | Time / d | Mass gain / (mgcm-2) | Oxide film thickness μm | p | Stress / GPa | | 360 ℃ | 3 | 0.1288 | 0.9 | - | - | | lithiated water | 14 | 0.1850 | 1.2 | -0.01318 | -2.2 | | 28 | 0.2285 | 1.5 | -0.01879 | -3.1 | | 42 | 0.2592 | 1.7 | -0.01695 | -2.8 | | 70 | 0.3020 | 2.0 | -0.02284 | -3.8 | | 98 | 0.3453 | 2.3 | -0.01491 | -2.5 | | 126 | 0.3785 | 2.5 | -0.01483 | -2.4 | | 154 | 0.5856 | 3.9 | -0.01113 | -1.8 | | 182 | 0.6808 | 4.5 | - | - | | 210 | 0.7290 | 4.9 | -0.01011 | -1.7 | | 238 | 0.7728 | 5.2 | -0.01171 | -1.9 | | 266 | 0.9000 | 6.0 | -0.01093 | -1.8 | | 294 | 1.0415 | 6.9 | -0.01022 | -1.7 | | 400 ℃ steam | 3 | 0.1700 | 1.1 | -0.01195 | -2.0 | | 14 | 0.2614 | 1.7 | -0.01521 | -2.5 | | 28 | 0.3242 | 2.2 | -0.01740 | -2.9 | | 42 | 0.3747 | 2.5 | -0.01303 | -2.1 | | 70 | 0.5163 | 3.4 | - | - | | 98 | 0.6232 | 4.2 | -0.00859 | -1.4 | | 126 | 0.7297 | 4.9 | - | - | | 154 | 0.8247 | 5.5 | -0.00981 | -1.6 | | 238 | 1.1614 | 7.7 | -0.00980 | -1.6 | | 266 | 1.1965 | 8.0 | -0.00929 | -1.5 |
|
|
|