激光原位制备硼化钛与镍钛合金增强钛基复合涂层
林英华, 雷永平, 符寒光, 林健
LASER IN SITU SYNTHESIZED TITANIUM DIBORIDE AND NITINOL REINFORCE TITANIUM MATRIX COMPOSITE COATINGS
LIN Yinghua, LEI Yongping, FU Hanguang, LIN Jian
表1
图4中各位置的EPMA分析结果
Position
Ti
B
Ni
Al
V
1
30.6~38.0
55.3~64.0
1.0~1.3
2.8~3.4
1.5~1.9
2
40.7~48.8
40.1~45.7
0.9~2.0
4.3~7.0
1.8~2.5
3
45.7~47.3
43.7~44.5
1.3~1.6
5.0~5.7
2.1~2.4
4
78.3~82.3
0
4.2~5.4
11.2~14.5
3.6~4.2
5
83.6~89.6
0
3.7~4.6
3.2~4.1
3.5~4.1