远青弧菌、硫酸盐还原菌及其混合菌种作用下 B10合金的海水腐蚀行为
|
|
魏仁超, 许凤玲, 蔺存国, 唐晓, 李焰
|
CORROSION BEHAVIOR OF B10 ALLOY EXPOSED TO SEAWATER CONTAINING VIBRIO AZUREUS, SULFATE-REDUCING BACTERIA, AND THEIR MIXTURE
|
|
WEI Renchao, XU Fengling, LIN Cunguo, TANG Xiao, LI Yan
|
|
| 表1 B10合金在4种腐蚀介质中的EIS解析参数 |
| Table 1 Parameters of electrochemical impedance of B10 alloy immersed in different mediums |
|
| Medium | Time | Rs | Ym | nm | Rm | Yt | nt | Rt | W, Y0 | | | Ω·cm2 | Ω-1·sn·cm-2 | | Ω·cm2 | Ω-1·sn·cm-2 | | Ω·cm2 | Ω-1·s5·cm-2 | | Sterile | 1 h | 19.34 | 296.2 | 0.7334 | 4198 | | | | 3.753×10-3 | | seawater | 1 d | 5.757 | 47.66 | 0.6027 | 1.696×104 | 104.5 | 0.6953 | 1.690×104 | 1.026×10-3 | | 2 d | 7.519 | 58.70 | 0.5651 | 1.354×104 | 28.98 | 0.7639 | 1.350×104 | 8.670×10-4 | | 4 d | 19.65 | 87.49 | 0.6399 | 1.211×104 | | | | 1.334×10-3 | | 7 d | 23.36 | 86.71 | 0.6271 | 1.438×104 | | | | 1.634×10-3 | | 13 d | 21.15 | 79.76 | 0.6341 | 1.497×104 | 28.54 | 0.7334 | 1.880×104 | 7.471×10-3 | | | Vibria | 1 h | 9.043 | 414.6 | 0.7363 | 1600 | | | | 5.695×10-3 | | azureus | 1 d | 10.11 | 183.4 | 0.8036 | 1837 | | | | 9.490×10-5 | | 2 d | 11.91 | 74.30 | 0.8993 | 2707 | | | | 3.870×10-5 | | 4 d | 10.75 | 68.97 | 0.9148 | 3551 | 31.59 | 0.6517 | 3.87×105 | 2.860×10-5 | | 7 d | 15.49 | 150.1 | 0.8001 | 9626 | 13850 | 1.000 | 3385 | 4.900×1013 | | 13 d | 13.40 | 166.1 | 0.8300 | 8877 | 17840 | 1.000 | 1778 | 2.640×1010 | | SRB | 1 h | 1.281 | 13.12 | 3.580×10-8 | 2.322 | 924.4 | 0.8188 | 80.31 | 6.960×10-4 | | 1 d | 3.112 | 976.7 | 0.8268 | 15.35 | 556.1 | 0.5131 | 1.771×104 | 5.660×10-5 | | 2 d | 3.194 | 180.7 | 1.000 | 1.606 | 1067 | 0.753 | 736.9 | 4.470×10-4 | | 4 d | 3.195 | 191.3 | 1.000 | 2.942 | 1141 | 0.7732 | 968.8 | 3.970×10-4 | | 7 d | 4.480 | 1858 | 0.7545 | 57.42 | 121.6 | 1.000 | 1517 | 3.480×10-4 | | 13 d | 4.019 | 1815 | 0.7586 | 70.39 | 206.4 | 0.9991 | 2235 | 2.480×10-4 | | Mixture | 1 h | 7.583 | 242.8 | 0.7946 | 56.38 | 202.7 | 0.7958 | 1.18×104 | 9.230×10-4 | | bacteria | 1 d | 6.595 | 185.3 | 0.8276 | 46.77 | 464.5 | 0.8278 | 1.66×104 | 1.254×10-3 | | 2 d | 4.713 | 164.3 | 0.8493 | 56.00 | 579.2 | 0.8370 | 2.41×104 | 1.256×10-3 | | 4 d | 5.450 | 176.3 | 0.8403 | 76.55 | 660.9 | 0.8603 | 4.35×104 | 3.266×10-3 | | 7 d | 9.947 | 217.1 | 0.8109 | 85.95 | 632.5 | 0.8749 | 5.94×104 | 2.330×10-3 | | 13 d | 5.322 | 235.3 | 0.8104 | 79.04 | 663.8 | 0.8690 | 8.33×104 | 2.420×106 |
|
|
|