表2 淬回火态UHCS, GCr15和SKF3钢中的球形残余碳化物体积分数、平均颗粒半径及残余奥氏体含量
Table 2 Volume fractions and average diameters of spherical residual carbide particles and retained austenite contents in quenched and tempered UHCS, GCr15 and SKF3 steels
Steel Carbide Mass fraction of C Volume fraction of
Volume fraction / % Average diameter / μm in martensite / % retained austenite / %
UHCS 4.47 0.46 0.18 7.5
GCr15 2.76 0.36 0.13 5.7
SKF3 2.74 0.28 0.11 6.3