表1 超高碳钢(UHCS), GCr15和SKF3钢的化学成分
Table 1 Chemical compositions of ultrahigh carbon steel (UHCS), GCr15 and SKF3 bearing steels
Steel C Si Mn Cr Al Mo Fe
UHCS 1.29 0.49 0.35 1.57 1.0 - Bal.
GCr15 1.00 0.28 0.19 1.61 - 0.078 Bal.