下贝氏体球墨铸铁在腐蚀介质中的磨粒磨损行为 |
|||||||||||||||
| 孙挺, 宋仁伯, 杨富强, 李亚萍, 吴春京 | |||||||||||||||
|
ABRASIVE WEAR BEHAVIOR OF LOWER BAINITE DUCTILE IRON IN CORROSION MEDIA |
|||||||||||||||
| SUN Ting, SONG Renbo, YANG Fuqiang, LI Yaping, WU Chunjing | |||||||||||||||
| 表1 粗糙度不同的下贝氏体球墨铸铁的腐蚀电位和腐蚀电流密度 | |||||||||||||||
| Table 1 Corrosion potential (Ecorr) and corrosion current density (icorr) of lower bainite ductile iron with different roughness Ra | |||||||||||||||
|
|||||||||||||||