PCB-HASL电路板在NaHSO3/Na2SO3溶液中的腐蚀电化学行为
|
|
丁康康, 肖葵, 邹士文, 董超芳, 赵瑞涛, 李晓刚
|
ELECTROCHEMICAL CORROSION BEHAVIOR OF PCB-HASL IN NaHSO3/Na2SO3 SOLUTION
|
|
DING Kangkang, XIAO Kui, ZOU Shiwen, DONG Chaofang, ZHAO Ruitao, LI Xiaogang
|
|
| 表2 在0.1 mol/L NaHSO3溶液中浸泡不同时间的PCB-HASL试样的EIS谱拟合结果 |
| Table 2 EIS fitting results of PCB-HASL immersed in 0.1 mol/L NaHSO3 solution for different times |
|
Time h | Rs Ω·cm2 | CPEf | n1 | Rf Ω·cm2 | L H·cm2 | RL Ω·cm2 | CPEdl | n2 | Rct Ω·cm2 | W S·s5·cm-2 | | 0.5 | 13.45 | 6.96×10-6 | 0.8687 | 1617 | 5.48×104 | 1.30×104 | 0.000078 | 0.8639 | 1014 | 0.004347 | | 1 | 14.80 | 7.62×10-6 | 0.8798 | 1291 | 7.79×104 | 1.41×104 | 0.000147 | 0.8144 | 627.6 | 0.007080 | | 2 | 14.09 | 1.23×10-5 | 0.8629 | 1057 | - | - | 0.000538 | 0.8778 | 265.2 | 0.012620 | | 3 | 14.33 | 1.57×10-5 | 0.8642 | 856.4 | - | - | 0.001199 | 0.9109 | 190.8 | 0.012550 | | 6 | 14.35 | 2.49×10-5 | 0.8748 | 769.4 | - | - | 0.001360 | 1.0000 | 198.1 | 0.012980 | | 12 | 15.02 | 3.90×10-5 | 0.8871 | 4231 | - | - | 0.000966 | 0.9675 | 721.2 | 0.005176 | | 24 | 11.83 | 1.07×10-4 | 0.9312 | 3229 | - | - | 0.000162 | 0.8475 | 7817 | - | | 36 | 19.26 | 1.02×10-4 | 0.9429 | 3435 | - | - | 0.000141 | 0.8429 | 9405 | - | | 72 | 14.15 | 1.30×10-4 | 0.9074 | 6213 | - | - | 0.000251 | 0.8375 | 8179 | - | | 120 | 18.86 | 7.82×10-4 | 0.7614 | 6418 | - | - | 0.000155 | 0.9063 | 10000 | - |
|
|
|