含Ag抗菌双相不锈钢组织及抗菌性能研究
|
|
向红亮, 郭培培, 刘东
|
MICROSTRUCTURE AND ANTIBACTERIAL PROPERTIES OF Ag-BEARING DUPLEX STAINLESS STEEL
|
|
XIANG Hongliang, GUO Peipei, LIU Dong
|
|
| 表4 与菌液作用不同时间的各试样的抗菌率 |
| Table 4 Antibacterial rates (R) of different specimens after different times in bacteria liquid |
|
| Specimen | Bacteria count / (cfu?mL-1) | | R / % | | 3 h | 24 h | | 3 h | 24 h | | A1 | 1.90×105 | >1.05×105 | | 84.8 | <91.6 | | A2 | 2.11×105 | >1.10×105 | | 83.1 | <91.2 | | A3 | 1.93×105 | >1.05×105 | | 84.6 | <91.6 | | B1 | 3.75×103 | <10 | | 99.7 | >99.9 | | B2 | 1.75×104 | <10 | | 99.6 | >99.8 | | B3 | 1.25×103 | <10 | | 99.9 | >99.9 | | C1 | 1.00×104 | <10 | | 99.2 | >99.9 | | C2 | 3.75×104 | <10 | | 99.4 | >99.9 | | C3 | 2.50×103 | <10 | | 99.8 | >99.9 | | D | >1.10×106 | 1.04×106 | | <11.3 | <16.7 | | 316L | 1.25×106 | 1.25×106 | | 0 | 0 |
|
|
|