含Ag抗菌双相不锈钢组织及抗菌性能研究
向红亮, 郭培培, 刘东
MICROSTRUCTURE AND ANTIBACTERIAL PROPERTIES OF Ag-BEARING DUPLEX STAINLESS STEEL
XIANG Hongliang, GUO Peipei, LIU Dong
表3
3和4中各相主要元素的含量
Fig.3
Contents of main elements in Fig.3 and Fig.4
Specimen
Phase
Cu
Ag
Ni
Cr
Fe
A
3
a
2.79
-
5.25
31.68
59.26
γ
7.55
-
8.75
22.61
61.06
Particle
8.89
41.87
2.24
19.11
24.86
B
3
a
2.36
0.03
5.40
27.56
58.56
γ
7.40
0.12
8.41
20.43
59.06
Particle
2.07
34.31
1.73
17.75
38.99