含Ag抗菌双相不锈钢组织及抗菌性能研究
|
|
向红亮, 郭培培, 刘东
|
MICROSTRUCTURE AND ANTIBACTERIAL PROPERTIES OF Ag-BEARING DUPLEX STAINLESS STEEL
|
|
XIANG Hongliang, GUO Peipei, LIU Dong
|
|
| 表2 5种试样中各相元素含量 |
| Table 2 Main chemical compositions of phases in different specimens |
|
| Specimen | Phase | Cr | Ni | Cu | Ag | Fe | | A1 | a | 30.19 | 5.34 | 2.39 | - | 58.64 | | γ | 23.31 | 8.31 | 5.25 | - | 60.54 | | Particle | 17.27 | 1.50 | 18.94 | 47.53 | 3.61 | | B1 | a | 29.01 | 5.49 | 2.74 | - | 59.89 | | γ | 23.32 | 7.98 | 5.92 | - | 61.17 | | Particle | 12.47 | 1.57 | 66.02 | 13.04 | 4.56 | | A3 | a | 29.09 | 5.10 | 2.45 | - | 59.49 | | γ | 22.28 | 8.68 | 5.31 | - | 61.52 | | Particle | 17.92 | 1.47 | 19.45 | 46.85 | 3.88 | | B3 | a | 28.66 | 5.41 | 2.32 | - | 59.38 | | γ | 23.22 | 8.11 | 7.49 | - | 59.57 | | C3 | a | 29.02 | 5.57 | 2.41 | - | 59.07 | | γ | 23.02 | 7.90 | 7.03 | - | 59.68 | | Particle | 12.53 | 1.68 | 65.10 | 12.93 | 4.42 |
|
|
|