含Ag抗菌双相不锈钢组织及抗菌性能研究
向红亮, 郭培培, 刘东

MICROSTRUCTURE AND ANTIBACTERIAL PROPERTIES OF Ag-BEARING DUPLEX STAINLESS STEEL
XIANG Hongliang, GUO Peipei, LIU Dong
表1 4种材料的化学成分
Table 1 Chemical compositions of four kinds of materials
Specimen C Si Mn S P Cr Ni Mo Cu Ag Fe
A1, A2, A3 0.03 0.54 0.74 0.002 0.03 25.91 5.91 1.95 3.16 0.135 Bal.
B1, B2, B3 0.03 0.53 0.79 0.002 0.03 25.74 5.89 1.93 3.14 0.121 Bal.
C1, C2, C3 0.03 0.52 0.79 0.002 0.03 25.82 5.78 1.94 3.16 0.128 Bal.
D 0.03 0.53 0.76 0.001 0.02 25.68 5.90 1.93 3.17 0 Bal.