镍基Inconel-718合金TIG焊部分熔化区组织变化*
|
|
叶欣, 华学明, 王敏, 楼松年
|
MICROSTRUCTURE EVOLUTION OF PARTIALLY MELTED ZONE OF TIG WELDING JOINT OF Ni-BASED INCONEL-718 SUPERALLOY
|
|
YE Xin, HUA Xueming, WANG Min, LOU Songnian
|
|
| 表2 Inconel-718合金铸态与均匀化的母材和PMZ区域元素含量与理论固液相线温度 |
| Table 2 Element contents and theoretical solidus and liquidus temperatures on as-cast and homogenization in base metal and PMZ zone for Inconel-718 superalloy |
|
| Type | Zone | Region | Mass fraction /% | Solidus | Liquidus | | | | Fe | Nb | K | K | | As-cast | Base metal | Laves | 16.19 | 26.02 | 1391 | 1621 | | Segregated γ | 17.30 | 8.17 | 1429 | 1586 | | Intradendriticγ | 24.87 | 2.69 | 1553 | 1668 | | Homogenization | Laves | 12.12 | 27.62 | 1376 | 1635 | | Segregated γ | 20.59 | 10.19 | 1423 | 1556 | | Intradendriticγ | 25.21 | 4.87 | 1462 | 1631 | | As-cast | PMZ | Laves | 21.54 | 26.30 | 1419 | 1625 | | Intradendriticγ | 29.25 | 1.91 | 1593 | 1693 | | Homogenization | Laves | 21.50 | 24.86 | 1430 | 1600 | | Intradendriticγ | 28.13 | 2.32 | 1572 | 1683 |
|
|
|