Loading...
Search for articles:
导航切换
Home
About AMSE
About AMSE
Editorial board
Coverage
Index In
Authors and reviewers
How to submit
Art instruction
Submission online
Instruction for reviewer
Reviewer login
Office login
Browse journal
Online first
Current issue
All past issues
Top cited
Top read
Top downloaded
Special issue
Order journal
Contact
AMSE-Springer
Archive
10 October 2024, Volume 37 Issue 10
Previous Issue
Next Issue
For Selected:
Download Citations
EndNote
Ris
BibTeX
Toggle Thumbnails
2024, 37 (10): 1643-1656. DOI:
10.1007/s40195-024-01728-7
Microstructure, Mechanical Properties and Corrosion Resistance of the Mo
0.5
V
0.5
NbTiZr
x
High-Entropy Alloys with Low Thermal Neutron Sections
Chao Xiang, En-Hou Han, Zhiming Zhang, Huameng Fu, Haifeng Zhang, Jianqiu Wang, Guodong Hu
Abstract
(
100
)
PDF
(
5376KB
)(
29
)
Rich HTML
(
8
)
2024, 37 (10): 1657-1666. DOI:
10.1007/s40195-024-01738-5
Atomistic Insights into the Irradiation Resistance of Co-Free High Entropy Alloy FeMnNiCr
Chunhui Wang, Lei Guo, Rui Li, Qing Peng
Abstract
(
83
)
PDF
(
1996KB
)(
11
)
Rich HTML
(
4
)
2024, 37 (10): 1667-1679. DOI:
10.1007/s40195-024-01748-3
Effects of Post-Heat Treatment and Carbide Precipitates on Strength-Ductility Balance of GH3536 Superalloy Prepared by Selective Laser Melting
Le Xia, Haijun Su, Quandong Hu, Yinuo Guo, Peixin Yang, Hongliang Gao, Minghui Yu, Min Guo, Zhuo Zhang, Lin Liu, Hengzhi Fu
Abstract
(
119
)
PDF
(
4853KB
)(
24
)
Rich HTML
(
11
)
2024, 37 (10): 1680-1688. DOI:
10.1007/s40195-024-01735-8
3D Graphene Nanosheets Crosslinked Core-Shell FeS
2
@N, S Co-Doped Porous Carbon for Improved Lithium/Sodium Storage Performance
Liang Chen, Lan-Yun Yang, Li-Ying Hu, Xu Liu, Chen-Xi Xu, Ying Liu, Wei Wang, Wen-Yuan Xu, Zhao-Hui Hou
Abstract
(
71
)
PDF
(
1798KB
)(
4
)
Rich HTML
(
3
)
2024, 37 (10): 1689-1702. DOI:
10.1007/s40195-024-01736-7
Phase Selection and Microstructure Evolution Dependance on Composition for Zr-Fe Eutectic Alloys
Dong-Dong Zuo, Jian Chang, Hai-Peng Wang
Abstract
(
77
)
PDF
(
6080KB
)(
12
)
Rich HTML
(
2
)
2024, 37 (10): 1703-1720. DOI:
10.1007/s40195-024-01746-5
Probing the Structural Stability, Mechanical, Electronic, and Thermodynamic Properties of Mg-Y-Zn Ternary Compounds via First-Principles Calculations
Wenjun Tian, Yunxuan Zhou, Tao Deng, Tao Chen, Jun Tan, Xianhua Chen, Fusheng Pan
Abstract
(
72
)
PDF
(
4644KB
)(
12
)
Rich HTML
(
4
)
2024, 37 (10): 1721-1734. DOI:
10.1007/s40195-024-01740-x
Effect of Rolling Temperature on the Mechanical Properties and Corrosion Behavior of Mg-Zn-Y-Nd Alloy Thin Sheets
Zhibin Liu, Guangya Zhu, Wenkai Li, Di Mei, Peihua Du, Yufeng Sun, Shijie Zhu, Shaokang Guan
Abstract
(
82
)
PDF
(
10740KB
)(
13
)
Rich HTML
(
7
)
2024, 37 (10): 1735-1751. DOI:
10.1007/s40195-024-01731-y
Implementation of Balanced Strength and Toughness of VW93A Rare-Earth Magnesium Alloy with Regulating the Overlapping Structure of Lamellar LPSO Phase and
$\beta^{\prime }$
Phase
Chao Wang, Xi Zhao, Yayun He, Dingxia Zheng
Abstract
(
69
)
PDF
(
9831KB
)(
12
)
Rich HTML
(
3
)
2024, 37 (10): 1752-1766. DOI:
10.1007/s40195-024-01737-6
First-Principles Calculations on Electronic Structure, Adhesion Strength, and Interfacial Stability of Mg(0001)/AlB
2
(0001) Nucleation Interface
Bo Li, Yonghua Duan, Mengnie Li, Lishi Ma, Shanju Zheng, Mingjun Peng
Abstract
(
69
)
PDF
(
5938KB
)(
10
)
Rich HTML
(
2
)
2024, 37 (10): 1767-1776. DOI:
10.1007/s40195-024-01734-9
Anodic Etching Surface Treatment and Antibacterial Properties of Ti-Cu
Zenglong Yan, Shuyuan Zhang, Ling Ren, Xizhuang Bai, Ke Yang, Xiang Wei
Abstract
(
59
)
PDF
(
3410KB
)(
9
)
Rich HTML
(
3
)
2024, 37 (10): 1777-1784. DOI:
10.1007/s40195-024-01733-w
A Novel Multiphase Stainless Steel with Ultra-Low Yield Ratio and High Ductility
Menghao Liu, Cuiwei Du, Yuewu Li, Xiaogang Li
Abstract
(
63
)
PDF
(
2782KB
)(
13
)
Rich HTML
(
5
)
2024, 37 (10): 1785-1792. DOI:
10.1007/s40195-024-01743-8
Untypical Electrochemical Corrosion Behavior of High-Nitrogen Austenitic Stainless Steel: Non-Pitting in Transpassivation
Qisi Wang, Qingchuan Wang, Xingxing Wang, Fan Liu, Ke Yang
Abstract
(
64
)
PDF
(
2573KB
)(
6
)
Rich HTML
(
5
)
2024, 37 (10): 1793-1808. DOI:
10.1007/s40195-024-01747-4
Functionalized Basalt Scales by Green Method for Higher Performance of Anticorrosion Coatings
Yichao Guo, Tianyue Jia, Jingsha Tan, Bo Zhang, Honglei Guo, Zhiyuan Feng, Bing Lei, Ping Zhang, Guozhe Meng
Abstract
(
82
)
PDF
(
7389KB
)(
12
)
Rich HTML
(
2
)
2024, 37 (10): 1809-1818. DOI:
10.1007/s40195-024-01742-9
Corrosion Behavior of High-Chromium Alloys in Molten LiCl-KCl Eutectic
Mengmeng Ji, Xin Li, Zihe Liu, Xiaoguang Yang, Xue Zhang, Ying Li