10 November 2023, Volume 36 Issue 11
Previous Issue
Next Issue
For Selected:
Download Citations
EndNote
Ris
BibTeX
Toggle Thumbnails
2023, 36 (11): 1749-1775. DOI:
10.1007/s40195-023-01593-w
Development of Phase-Field Modeling in Materials Science in China: A Review
Yuhong Zhao, Hui Xing, Lijun Zhang, Houbing Huang, Dongke Sun, Xianglei Dong, Yongxing Shen, Jincheng Wang
Abstract
(
249
)
PDF
(
12260KB
)(
141
)
Rich HTML
(
31
)
2023, 36 (11): 1776-1790. DOI:
10.1007/s40195-023-01598-5
A Hot Cracking Initiation Criterion Based on Solidification Liquid Film Characteristic and Microstructure
Ming Su, Wentao Zheng, Chunyu Yue, Bowen Zheng, Xiaojiao Zuo, Mengyuan He, Xiaoguang Yuan
Abstract
(
101
)
PDF
(
3114KB
)(
44
)
Rich HTML
(
8
)
2023, 36 (11): 1791-1804. DOI:
10.1007/s40195-023-01591-y
Phase-Field Lattice-Boltzmann Study for α-Mg Dendrite Growth of Mg-5wt%Zn Alloy with Forced Convection
Wei-Peng Chen, Hua Hou, Yun-Tao Zhang, Wei Liu, Yu-Hong Zhao
Abstract
(
93
)
PDF
(
6606KB
)(
21
)
Rich HTML
(
7
)
2023, 36 (11): 1805-1821. DOI:
10.1007/s40195-023-01594-9
Dual Strengthened Control of Recrystallization Behavior on CVCDE Magnesium Alloy Containing Characteristic Structure
Nan Bian, Feng Li, Wentao Niu, Chao Li, Yuanqi Li
Abstract
(
91
)
PDF
(
11783KB
)(
22
)
Rich HTML
(
9
)
2023, 36 (11): 1822-1832. DOI:
10.1007/s40195-023-01590-z
Effect of Extrusion Temperature on the Mechanical Properties and Corrosion Behavior of LZ91 Alloys
Xuejian Wang, Huaqiang Xiao, Keqiang Su, Bo Lin, Tongmin Wang, Enyu Guo
Abstract
(
99
)
PDF
(
3011KB
)(
18
)
Rich HTML
(
7
)
2023, 36 (11): 1833-1843. DOI:
10.1007/s40195-023-01581-0
Developing Zn-1.5Mg Alloy with Simultaneous Improved Strength, Ductility and Suitable Biodegradability by Rolling at Room Temperature
Ziyue Xu, Huan Liu, Guangyang Hu, Xiaoru Zhuo, Kai Yan, Jia Ju, Wenkai Wang, Hang Teng, Jinghua Jiang, Jing Bai
Abstract
(
117
)
PDF
(
4485KB
)(
28
)
Rich HTML
(
7
)
2023, 36 (11): 1844-1856. DOI:
10.1007/s40195-023-01589-6
Latent Heat of TB18 Titanium Alloy during β to α Phase Transition by DSC and First-Principles Methods
Yan-Di Jia, Shuo Cao, Ying-Jie Ma, Sen-Sen Huang, Feng-Ying Qin, Shao-Qiang Li, Wei Xiang, Qian Wang, Qing-Miao Hu, Bo Li, Jia-Feng Lei, Jing Xie, Xiang-Hong Liu, Rui Yang
Abstract
(
98
)
PDF
(
8711KB
)(
37
)
Rich HTML
(
6
)
2023, 36 (11): 1857-1869. DOI:
10.1007/s40195-023-01588-7
Intermediate Temperature Fatigue Induced Precipitation and Associated Corrosion in CrMnFeCoNi High Entropy Alloy
Tiezhuang Han, Jing Wang, Bo Li, Shuang Li, Kaisheng Ming, Fucheng Wang, Bin Miao, Shijian Zheng
Abstract
(
125
)
PDF
(
4017KB
)(
23
)
Rich HTML
(
9
)
2023, 36 (11): 1870-1882. DOI:
10.1007/s40195-023-01606-8
Thermal Deformation Behavior and Processing Map of a Novel CrFeNiSi
0.15
Medium Entropy Alloy
Hongbin Zhang, Kang Chen, Zhongwei Wang, Haiping Zhou, Chengcheng Shi, Shengxue Qin, Jie Liu, Tingjun Lv, Jian Xu
Abstract
(
103
)
PDF
(
4402KB
)(
27
)
Rich HTML
(
7
)
2023, 36 (11): 1883-1892. DOI:
10.1007/s40195-023-01599-4
Thickness-Dependent Microstructure and its Effect on Anisotropic Mechanical Properties of Duplex Stainless Steel 2205 Multi-pass Welded Joints
Zhilong Dong, Xue-Fang Xie, Jingwen Li, Yu Wan
Abstract
(
93
)
PDF
(
6539KB
)(
21
)
Rich HTML
(
8
)
2023, 36 (11): 1893-1908. DOI:
10.1007/s40195-023-01600-0
Protective Coatings Containing ZnMOF-BTA Metal-Organic Framework for Active Protection of AA2024-T3
Izuchukwu K. Nwokolo, Hongwei Shi, Paul C. Uzoma, Sharjeel Ahmed, Jiwen Li, Fuchun Liu
Abstract
(
103
)
PDF
(
5540KB
)(
17
)
Rich HTML
(
8
)
2023, 36 (11): 1909-1923. DOI:
10.1007/s40195-023-01596-7
Mechanical Properties and Oxidation Behaviors of Self-Healing SiC
f
/SiC-SiBCN Composites Exposed to H
2
O/O
2
/Na
2
SO
4
Environments
Suya Ji, Bin Liang, Chenglong Hu, Shengyang Pang, Rida Zhao, Jian Li, Sufang Tang
Abstract
(
113
)
PDF
(
4083KB
)(
12
)
Rich HTML
(
5
)
2023, 36 (11): 1924-1924. DOI:
10.1007/s40195-023-01592-x
Correction to: Influence of Electroshocking Treatment on Microstructure and Mechanical Properties of Ti-6.5Al-3.5Mo-1.5Zr-0.3Si Thin-Wall Specimen Manufactured by Laser Melting Deposition
Yan Wen, Xuan Sun, Jian Zhou, Bingliang Liu, Haojie Guo, Yuxin Li, Fei Yin, Liqiang Wang, Lechun Xie, Lin Hua
Abstract
(
75
)
PDF
(
372KB
)(
20
)
Rich HTML
(
13
)
E-mail alert