Corrosion Science and Protection Technology
Home
IMR Journals
Subscription
Advertisement
Contact us
中文
Search
Citation
Fig/Tab
adv Search
Just Accepted
|
Current Issue
|
Archive
|
Featured Articles
|
Special Issue
|
Most Read
|
Most Downloaded
|
Most Cited
ISSN 1002-6495
CN 21-1264/TQ
Started in 1989
About the Journal
»
About Journal
»
Editorial Board
»
Indexed in
»
Fund
»
Rewarded
Authors
»
Online Submission
»
Guidelines for Authors
»
Copyright Agreement
Reviewers
»
Guidelines for Reviewers
»
Online Peer Review
»
Online Editor Work
Office
»
Editor-in-chief
»
Office Work
Current Issue
, Volume 9 Issue 4
Previous Issue
Next Issue
For Selected:
View Abstracts
Download Citations
EndNote
Reference Manager
ProCite
BibTeX
RefWorks
Select
ELECTROCHEMICAL SCANNING TUNNELING MICROSCOPE STUDIES OF INITIAL PITTING CORROSION IN 18/8 STAINLESS STEEL
LIN Changjian; XIE Zhaoxiong; TIAN Zhaowu (Institute of Physical Chemistry; Department of Chemistry State Key Lab for Physical Chemistry of the Solid Surface; Xiamen University; Xiamen 361005)
Corrosion Science and Protetion Technology, 1997,
9
(4): 3-8.
Abstract
PDF
(1050KB) (
884
)
The surface topographies of stainless steel in an early stage of pitting corrosion were imaged by a home made electrochemical scanning tunneling microscope (ECSTM). The influences of potential, chloride and time on the surface topographics were examined i
References
|
Related Articles
|
Metrics
Select
THE INFLUENCE OF In3+ ON THE NEGATIVE DIFFERENCE EFFECT OF ALUMINIUM
XU Gang; LIN Haichao; ZHANG Jianqing1; CAO Chu'nan (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015) (1 Department of Chemistry; Zhejiang University
Corrosion Science and Protetion Technology, 1997,
9
(4): 15-19.
Abstract
PDF
(909KB) (
887
)
The electrochemical behavior of Aluminum in 0.5mol/L NaCl solution was studied by potentiodynamic method and potentiostatic hydrogen gathering measurement. When high hydrogen evolution overpotential metal ion In3+ was added in the solution , the active
References
|
Related Articles
|
Metrics
Select
APPLICATION OF KELVIN PROBE TECHNIQUE TO THE STUDY OF CORROSION OF WELDED STAINLESS STEELS
ZOU Feng; Dominigue Thierry (1); HAN Wen′an; HAN Wei (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015) REN Xiaoshan; HU Xizhang; CHEN Xiaojun (Lutianh
Corrosion Science and Protetion Technology, 1997,
9
(4): 20-24.
Abstract
PDF
(805KB) (
1049
)
The surface profile and the potential difference distributions over welded stainless steels were measured by using scanning Kelvin probe technigue.A good relation was found between the potential distributon and the corrosion behavior of the specimens expo
References
|
Related Articles
|
Metrics
Select
A STUDY ON SELECTION OF KEY FACTORS IN SOIL CORROSION MODELING
WENG Yongji; LI Xiangyi (University of Petroleum; Beijing 102200)
Corrosion Science and Protetion Technology, 1997,
9
(4): 25-29.
Abstract
PDF
(920KB) (
904
)
In this paper the classification of corrosion factors and the selection of key parameters in corrosion modeling were studied. Based on the correlation coefficient matrix recreated from original data set, the classification diagram of corrosion factors wa
References
|
Related Articles
|
Metrics
Select
EFFECT OF POLARIZATION AND FREQUENCY ON CRACK PROPAGATION BEHAVIOR OF A537 STEEL IN 3.5% NaCl SOLUTION
WANG Jianqiu; LI Jin; KE Wei (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015)
Corrosion Science and Protetion Technology, 1997,
9
(4): 30-36.
Abstract
PDF
(2012KB) (
915
)
The effect of polarization and frequency on the crack propagation behavior including crack propagation rate(CPR) and fracture surface was studied. The results showed that in A537/3.5%NaCl active system CPR increased with the decrease of frequency under s
References
|
Related Articles
|
Metrics
Select
THE INHIBITION OF MANNICH BASES
KUANG Fugui; ZHAO Wentao; QIAO Shengying; YAO Lu'an (Department of Environmental Science; Wuhan University; Wuhan 430072)
Corrosion Science and Protetion Technology, 1997,
9
(4): 37-40.
Abstract
PDF
(551KB) (
1043
)
Seven pure Mannich bases were synthesized, their corrosion inhibition for 20# carbon steel in 1 mol/L HCl solution was examined by using weight loss, polarization resistance and polarization curve measurements. The effect of the chemical structure of Ma
References
|
Related Articles
|
Metrics
Select
PRELIMINARY STUDY OF INTERGRANULAR CORROSION SUSCEPTIBILITY OF AUSTENITIC STAINLESS STEEL BY CPE METHOD
ZHANG Wei; TIAN Hong; LI Jiuqing (USTB; the Opening Corrosion Erosion & Surface Technology Laboratory of Metallurgical Ministry; Beijing 100083)
Corrosion Science and Protetion Technology, 1997,
9
(4): 41-45.
Abstract
PDF
(986KB) (
850
)
The susceptibility to intergranular corrosion of 304L austenitic stainless steel was studied by CPE (constant potential etching) method. Then the results of CPE method were varified by EPR (electrochemical potential kineti
References
|
Related Articles
|
Metrics
Select
SERS AND ELECROCHEMICAL STUDIES OF ADSORPTION OF THIOUREA AND UREA AT SILVER ELECTRODE
XU Haibo; YU Jiakang; DONG Junhua; LIN Haichao; CAO Chu'nan (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015)
Corrosion Science and Protetion Technology, 1997,
9
(4): 46-51.
Abstract
PDF
(960KB) (
982
)
Adsorption behaviors of thiourea and urea at the silver electrode in sulphuric acid solution were investigated using polarization curves and Raman spectroscopy. It was shown that thiourea took part in the reaction of anodic dissolution of siver,and
References
|
Related Articles
|
Metrics
Select
PROGRESS IN RESEARCH OF INHIBITORS
LIN Haichao (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Portection of Metals; The Chinese Academy of Sciences; Shenyang 110015)
Corrosion Science and Protetion Technology, 1997,
9
(4): 52-57.
Abstract
PDF
(1361KB) (
1759
)
The results of research on inhibitors and their action mechanisms in recent years were reviewed. The following aspects were mainly discussed: the inhibitive action mechanism of inhibitors for SCC, the inhibitive action of thiourea and its derivatives, cin
References
|
Related Articles
|
Metrics
Select
INVESTIGATION AND DRAINAGE OF STRAY CURRENT ON AN OIL PIPELINE
ZHAO Jian; ZHANG Lihua; ZHAO Quan; PU Yuping 1;CHANG Shouwen (Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015) (1 Central Iron & Steel Research Institute; MMI; Beijing 100081) WANG Lianxue; ZHOU Yajun;
Corrosion Science and Protetion Technology, 1997,
9
(4): 58-62.
Abstract
PDF
(961KB) (
1010
)
By measuring pipeline to soil potential,potential gradient and stray current direction, an investigation of stray current on an oil pipeline showed that the stray current interference was very large. Therefore, a sacrificial anode drainage was applied
References
|
Related Articles
|
Metrics
Select
THE ANALOGUE TEST RESEARCH OF THE SACRIFICIAL ANODE PROTECTION AT A SEAWATER COOLER
WANG Haijiang; HU Shutao\ \ \ \ \ \ \ \ YANG Shiwei \ \ \ (Shanghai University; Shanghai 200072)\ \ (Harbin Engineering University;Harbin 150001)
Corrosion Science and Protetion Technology, 1997,
9
(4): 63-66.
Abstract
PDF
(803KB) (
903
)
The seawater cooler of a exhaust silencer was manufactured with 316L stainless steel and protected with zinc alloy sacrificial anodes . The potential distribution of the cooler and the weightloss of the sacrificial anodes were determined on a 1∶1 model wh