Corrosion Science and Protection Technology
Home
IMR Journals
Subscription
Advertisement
Contact us
中文
Search
Citation
Fig/Tab
adv Search
Just Accepted
|
Current Issue
|
Archive
|
Featured Articles
|
Special Issue
|
Most Read
|
Most Downloaded
|
Most Cited
ISSN 1002-6495
CN 21-1264/TQ
Started in 1989
About the Journal
»
About Journal
»
Editorial Board
»
Indexed in
»
Fund
»
Rewarded
Authors
»
Online Submission
»
Guidelines for Authors
»
Copyright Agreement
Reviewers
»
Guidelines for Reviewers
»
Online Peer Review
»
Online Editor Work
Office
»
Editor-in-chief
»
Office Work
Current Issue
, Volume 10 Issue 2
Previous Issue
Next Issue
For Selected:
View Abstracts
Download Citations
EndNote
Reference Manager
ProCite
BibTeX
RefWorks
Select
RESEARCH AND APPLICATION OF POTENTIAL DISTRIBUTION MODELLING IN CATHODIC PROTECTION
LI Xiangyi; WENG Yongji (University of Petroleum; Beijing 102200)
Corrosion Science and Protetion Technology, 1998,
10
(2): 4-10.
Abstract
PDF
(1282KB) (
881
)
The currents of cathodic protection(CP) sysytem were analysed into several parts, namely: currents along the protected equipments; currents from anodes to ground; and currents from ground to protected equipments. According to the electric field theory of
References
|
Related Articles
|
Metrics
Select
PREPARATION, STRUCTURE AND HIGH TEMPERATURE PROPERTIES OF THERMAL BARRIER COATINGS BY LASER CLADDING
GAO Yang *; LIANG Yong; SHI Changxu (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015) (* Beijing Institute of Aeronautical Materials; Beijing 100095)
Corrosion Science and Protetion Technology, 1998,
10
(2): 11-16.
Abstract
PDF
(1501KB) (
938
)
A new type of thermal barrier coating is being developed for aircraft gas turbine blades by laser cladding on superalloy substrates. During rapid melting and solidification in laser processing, an oriented epitaxial growth, closely packed columnar structu
References
|
Related Articles
|
Metrics
Select
ELECTROCHEMICAL CORROSION BEHAVIOUR OF VARIOUS Ni COATING/CARBON STEEL BILAYER IN OXYGEN FREE WATER AT HIGH TEMPERATURES
WANG Xuefen; WEI Baoming (Department of Applied Chemistry; Nanjing University of Chemical Technology;Nanjing 210009 )
Corrosion Science and Protetion Technology, 1998,
10
(2): 17-22.
Abstract
PDF
(910KB) (
921
)
The electrochemical corrosion behaviour of electroless amorphous Ni P coating/carbon steel substrate and electro deposited nanocrystalline Ni coating/carbon steel substrate were studied by linear polarization, potentiostatic curve and AC impe
References
|
Related Articles
|
Metrics
Select
CYCLIC OXIDATION BEHAVIOUR OF THE SPUTTERED MICROCRYSTALLINE COATING OF LDZ125 SUPERALLOY AT 1000℃
ZHANG Jie; LOU Hanyi (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015)
Corrosion Science and Protetion Technology, 1998,
10
(2): 23-27.
Abstract
PDF
(1229KB) (
792
)
The sputtered LDZ125 coating producted by planar magnetron sputtering technique has homogeneous structure and very fine grain size(less than 100 nm) consisting of γ phase, while the cast alloy is composed of γ,γ' and carbides. The cyclic oxidation resista
References
|
Related Articles
|
Metrics
Select
THE ELECTROCHEMICAL BEHAVIOR OF CARBON STEEL ELECTRODE IN FLOWING 3.5% NaCl SOLUTION
YONG Xingyue; XU Ruifen; LI Huanwen; LIN Yuzhen (Dept. of Applied Chemistry;Beijing University of Chemical Technology; Beijing 100029)
Corrosion Science and Protetion Technology, 1998,
10
(2): 28-33.
Abstract
PDF
(1286KB) (
947
)
The electrochemical impedance spectroscopy of carbon steel in flowing 3.5% NaCl solution was studied. The experimental results showed that: the Nyquist plots for carbon steel in flowing single or double phase solution were single capacitive loops. With i
References
|
Related Articles
|
Metrics
Select
GALVANIC CORROSION BEHAVIOR BETWEEN GRAPHITE/EXPOXY COMPOSITE MATERIAL(GECM) AND METAL
HU Yanling; LI Di; GUO Baolan (Beijing Astronautic and Aeronautic University; Beijing 100083)
Corrosion Science and Protetion Technology, 1998,
10
(2): 34-38.
Abstract
PDF
(917KB) (
927
)
The behavior of galvanic corrosion between graphite/epoxy conposites(GECM)and metals(LD10,YLD10,H62,1Cr18Ni9Ti) at different temperatures (28℃,35℃,45℃,65℃) was evaluated by galvanic couple tests for 30 days. Results indicated that significant galvanic cor
References
|
Related Articles
|
Metrics
Select
THE ALKALINE FILM FORMING TECHNOLOGY OF RARE EARTH CONVERSION FILM ON ALUMINUM AND ITS ALLOY
LI Jiuqing; Tian Hong; LU Cuiying (The Opening Corrosion Erosion & Surface Technology Laboratorey of the Metallurgical Ministry; University of Science and Technology of Beijing; Beijing 100083)
Corrosion Science and Protetion Technology, 1998,
10
(2): 39-43.
Abstract
PDF
(919KB) (
838
)
The performance of conversion films containing rare earth element on aluminum and its alloys has been studied by linear polarization technique,polarization curve measuring,and neutral salt spray test.The test results revealed that: the uniform corrosion r
References
|
Related Articles
|
Metrics
Select
REVIEW ON CORROSION PERFORMANCE TITANIUM BIOMEDICAL MATERIALS
MOU Zhanqi; LIANG Chenghao (Dalian University of Technology; Dalian 116012)
Corrosion Science and Protetion Technology, 1998,
10
(2): 44-49.
Abstract
PDF
(1031KB) (
926
)
The corrosion resistance of Ti biomedical materials in body fluids was reviewed. The main corrosion types including local corrosion, fretting corrosion, corrosion fatigue and stress corrosion cracking were introduced. It was showed that the titanium and t
References
|
Related Articles
|
Metrics
Select
TITANIUM SUPPORTED IRIDIUM DIOXIDE ELECTRODE IN CATHODIC PROTECTION
XIANG Qian; HUANG Yongchang(1); JIANG Xuewen(1); ZHAO Guangrui(1) (The Research Institituty of No.3 Harbour Engineering Bureau; Shanghai 200032) (1 Shanghai Jiao Tong University; Shanghai 200024)
Corrosion Science and Protetion Technology, 1998,
10
(2): 50-54.
Abstract
PDF
(926KB) (
879
)
IrO 2 SnO 2/Ti and IrO 2 PdO x SnO 2/Ti electrodes were made by the thermal decomposition technique in air. The electrochemical behaviors of the anodes were studied by polarization curves,cyclic voltammetry curves and electrolytical experimentation in fre
References
|
Related Articles
|
Metrics
Select
ELECTRICAL DRAINAGE AND CATHODIC PROTECTION OF BURIED WATER PIPELINE
LIANG Chenghao ; WANG Jie 1 ; LI Shuying ; JIANG Yeliang (Dalian Unversity of Technology; Dalian 116012) (1 Anshan Iron and Steel Research; Anshan 114001)
Corrosion Science and Protetion Technology, 1998,
10
(2): 55-58.
Abstract
PDF
(668KB) (
992
)
The stray current corrosion of buried water pipeline of a plant at Anshan was prospected and analyzed. The direct electrical drainage protection and cathodic protection methods were designed . During 6 years in service , it was found that the united prote
References
|
Related Articles
|
Metrics
Select
SCC ON AN AUSTENITIC STAINLESS STEEL WELDED STRUCTURE DUE TO POOR WELDING QUALITY
PAN Xide; SHEN Fenggang; DONG Junming; XUE Jin (Xi'an Jiaotong University; Xi'an 710049)
Corrosion Science and Protetion Technology, 1998,
10
(2): 59-62.
Abstract
PDF
(804KB) (
909
)
316L stainless steel is a kind of material with good corrosion resistance, but its properties of anti SCC are considerably affected by assembling quality, especially by welding quality. The failure on the heat affected zone (HAZ) in a 316L stainless stee