EFFECT OF GROWTH ANGLE AND SOLIDIFICATION RATE ON THE FLOATING ZONE STABILITY FOR PROCESSING OF HIGH-TEMPERATURE PURE METALS

  • Shuangming LI ,
  • Zhenbo GENG ,
  • Rui HU ,
  • Yi LIU ,
  • Ximing LUO
Expand
  • 1 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072
    2 Kunming Institute of Precious Metals, Kunming 650106

Revised date: 2014-07-18

  Online published: 2015-01-25

Supported by

Supported by National Natural Science Foundation of China-Yunnan Province Joint Fund (No.U1202273)

Abstract

The height of floating zone and molten zone instability for five pure metals including Nb, W, Ta, Mo, and Ir with high melting points is investigated using electron beam floating zone method (EBFZM). The results show that the height level of floating zone for these five metals are in order with the sequence of Nb>Mo>W>Ta>Ir. The crystal growth angles for these metals are in the range of 8°~13° and the sample in large size can be developed by EBFZM as the growth angle is found not to be zero. Meanwhile, the actual growth angles are related with the interface growth mechanism. For continuous growth mechanism, the growth angles vary slightly with the solidification rate for rough interface, and for dislocation growth mechanism, the growth angles decrease with increasing the solidification rate. If faceting growth mechanism prevails, the growth angles drop remarkably at a low solidification rate and further increase with increasing the solidification rate. Additionally, by employing EBFZM growth of Ir and Mo pure metals, a solidification rate approaching 1 mm/min is available for controlling the growth angle and the height of floating zone. These calculations fit well with the experimental results of Mo single crystal prepared by EBFZM.

Cite this article

Shuangming LI , Zhenbo GENG , Rui HU , Yi LIU , Ximing LUO . EFFECT OF GROWTH ANGLE AND SOLIDIFICATION RATE ON THE FLOATING ZONE STABILITY FOR PROCESSING OF HIGH-TEMPERATURE PURE METALS[J]. Acta Metall Sin, 2015 , 51(1) : 114 -120 . DOI: 10.11900/0412.1961.2014.00400

References

[1] Zee R H, Xiao Z, Chin B A, Liu J. J Mater Proc Technol, 2001; 113: 75
[2] Baars R E. Evolution of Refractory Metals and Alloys. Pennsyvania: The Minerals, Metals & Materials Society, 1994: 185
[3] Ohriner E K. Platinum Met Rev, 2008; 52: 186
[4] Verstraete M J, Christpehe C J. Appl Phys Lett, 2005; 86: 191917
[5] Glebovsky V G, Semonov V N. Int J Refractory Met Hard Mater, 1993-1994; 12: 295
[6] Glebovsky V G, Semonov V N. High Temp Mater Proc, 1995; 14: 121
[7] Hu Z W, Li Z K, Zhang Q, Zhang T J, Zhang J L, Yin T. Rare Met Mater Eng, 2007; 36: 367
[7] (胡忠武, 李中奎, 张 清, 张廷杰, 张军良, 殷 涛. 稀有金属材料与工程, 2007; 36: 367)
[8] Glebovsky V G, Semonov V N, Lomeko V V. J Crystal Growth, 1989; 98: 487
[9] Duffar T. Crystal Growth Processes Based on Capillarity. Chichester: John Wiley & Sons Ltd, 2010: 204
[10] Virozub A, Rasin I G, Brandon S. J Cryst Growth, 2008; 310: 5416
[11] Satunkin G A. J Cryst Growth, 2005; 255: 170
[12] Johns L E, Narayanan R. Interfacial Instability. New York: Springer-Verlag, Inc., 2002: 8
[13] Keene B J. Int Mater Rev, 1993; 38: 157
[14] Jiang Q, Lu H M. Surf Sci Rep, 2008; 63: 427
[15] Wang H. Master Thesis, Northwestern Polytechncial University, Xi′an, 2007: 23
[15] (王 红. 西北工业大学硕士学位论文, 西安, 2007: 23)
[16] Weinstein O, Brandon S. J Cryst Growth, 2004; 268: 299
[17] Ludge A, Riemann H, Wunscher M, Behr G, Loser W, Muiznieks A, Croll A. In: Duffar T ed., Crystal Growth Processes Based on Capillarity. Chichester: John Wiley & Sons Ltd, 2010: 203
[18] Min N B. Physical Fundamentals of Crystal Growth. Shanghai: Shanghai Science & Technology Press, 1982: 398
[18] (闵乃本. 晶体生长的物理基础. 上海: 上海科学技术出版社, 1982: 398)
[19] Zhang Q, Li Z K, Zhen Y Z, Zhang J L, Hu Z W, Zhang T J, Yin T, Ding X F, Ding X. Rare Met Mater Eng, 2005; 34: 1498
[19] (张 清, 李中奎, 郑玉柱, 张军良, 胡忠武, 张廷杰, 殷 涛, 丁学峰, 丁 旭. 稀有金属材料与工程, 2005; 34: 1498)
[20] Tiller W A. The Science of Crystallization:Microscopic Interfacial Phenomena. Cambridge: Cambridge University Press, 1991: 87
Outlines

/

〈 〉