Abstract

Chalcopyrite (CuFeS2) is the most common copper bearing sulfide in the natural world, and it is also the most widespread copper ore in the world. Pyrometallurgy is used to extract copper from chalcopyrite as main industrial method. However, environmentally friendly metallurgy is advocated because of increasingly serious environmental pollution. The bacterial metallurgy is considered a new clean smelting technology to deal with low--grade and complicated composition metal resources because of short flow, simple operation, low investment and friendly environment. In the process of bioleaching, the formation of oxide film on the chalcopyrite crystal surface hindered the rapid dissolution of chalcopyrite and restricted the large-scale application of copper bioleaching. It is concluded that the oxide film inhibits material exchange between chalcopyrite and leaching liquid on the surface of the chalcopyrite and depresses its leaching rate significantly. In the paper, the advanced surface analysis technologies, such as SEM, XRD and X-ray photoelectron spectroscopy (XPS) are used to observe and analysis the surface layer in the bacterial leaching process. It is studied for the formation of bio-oxide film on the natural chalcopyrite crystal surface, in order to reveal the passivation mechanism of chalcopyrite bioleaching. Through the observation of the microcosmic morphology characteristic changes of chalcopyrite during bioleaching, different chemical composition analysis of surface oxide layer in the different bacterial oxide phase were studied. The results show that the insoluble oxide film inhibits material exchange between chalcopyrite and leaching liquid on the surface of the chalcopyrite and depresses its leaching rate significantly. The results show that the rudiments of oxide film are formed on the surface of chalcopyrite after leaching for 72 h. The oxide layer with certain thickness is formed after 96 h, and the passivation is produced. The compact film is formed after 168 h because bacterial corrosion spots and rillsare formed on the surface of chalcopyrite, and it is begun to produce serious passivation. The variation of chemical state of sulfur element is S2-→S0→S4+→S6+. The reaction product, including iron deficiency copper sulfide
Cu$_{1-x}$Fe$_{1-y}$S$_{z}$($x iron oxide (Fe(III)-oxide), iron hydroxide oxide (Fe(III)-O-OH) and
jarosite (KFe3(SO4)2(OH)6) are formed on the surface
of chalcopyrite in order in the bioleaching process. The chalcopyrite
passive film formed is caused by the stable and compact layer whose main
composition is jarosite, and it produces strong passivation effects on the
chalcopyrite bacterial leaching.

Cite this article

YANG Hong-Yang , PAN Hao-Dan , TONG Lin-Lin , LIU Yuan-Yuan . FORMATION PROCESS OF BIOLOGICAL OXIDE FILM ON CHALCOPYRITE CRYSTAL SURFACE[J]. Acta Metall Sin, 2012 , 48(9) : 1145 -1152 . DOI: 10.3724/SP.J.1037.2012.00279

References

[1] BrierleyJ A. FEMS Microbiol Lett, 1990; 75: 287

[2] Rohwerder T, Gehrke T, Kinzler K, Sand W. Appl Microbiol Biotechnol, 2003; 63: 239

[3] Dutrizac J E. Metall Trans, 1978; 9B: 431

[4] Petersen J, David G D. Hydrometallurgy, 2006; 83: 40

[5] Morin D, Lips A, Pinches T, Huisman J, Frias C, Norberg A, Forssberg E. Hydrometallurgy, 2006; 83: 69

[6] Bestamin O, Erkan S, Pauliina N, Anna H K, Jaakko A P. Hydrometallurgy, 2007; 88: 67

[7] Leahy MJ, DavidsonM R, SchwarzMP. Hydrometallurgy, 2007; 85: 24

[8] Cecilia S D, Pedro A G P, Lorena V E G, V´?ctor J Z A, Danny C, Emilio O C. Hydrometallurgy, 2005; 80: 241

[9] Rebecca B H, Peter D F, Jason J P. Hydrometallurgy, 2006; 83: 229

[10] Parker A, Klauber C, Kougianos A, Watling H R, van Bronswijk W. Hydrometallurgy, 2003; 71: 265

[11] Lopez–Juarez A, Gutierrez–Arenas N, Rivera–Santill´an R E. Hydrometallurgy, 2006; 83: 63

[12] Brierley J A, Brierley C L. Hydrometallurgy, 2001; 59: 233

[13] Watling H R. Hydrometallurgy, 2006; 84: 81

[14] Mousavi S M, Yaghmaei S, Vossoughi M, Jafari A, Hoseini S A. Hydrometallurgy, 2005; 80: 139

[15] Rodr?ques Y, Ballester A, Bl´azques M L, Gonzales F, Munoz J A. Hydrometallurgy, 2003; 71: 37

[16] Hackl R P, Dreisinger D B, Peters E, King J A. Hydrometallurgy, 1995; 39: 25

[17] Harmer S L, Thomas J E, Fornasiero D, Gerson A R. Geochim Cosmochim Acta, 2006; 70: 4392

[18] Liang C L, Xia J L, Yang Y, Nie Z Y, Qiu G Z. Chin J Nonferrous Met, 2012; 22: 265

(梁长利, 夏金兰, 杨益, 聂珍媛, 邱冠周. 中国有色金属学报, 2012; 22: 265)

[19] Xia L X, Tang L, Xia J L, Yin C, Cai L Y, Zhao X J, Nie Z Y, Liu J S, Qiu G Z. Trans Nonferrous Met Soc China, 2012; 22: 192

[20] Bevilaqua D, Diezperez I, Fugivara C S, Sanz F, Benedetti A V, Garcia Jr O. Bioelectrochemistry, 2004; 64: 79

[21] Yao G C, Wen J K, Gao H Z, Wang D Z. J Cent South Univ (Sci Technol), 2010; 41: 1234

(姚国成, 温建康, 高焕芝, 王淀佐. 中南大学学报(自然科学版), 2010; 41: 1234)

[22] Ahmadi A, Schaffie M, Manafi Z, Ranjbar M. Hydrometallurgy, 2010; 104: 99

[23] Third K A, Cordruwisch R, Watling H R. Hydrometallurgy, 2000; 57: 225

[24] Silverman M, Lundgren D. J Bacteriol, 1959; 77: 642

[25] Pan H D, Yang H Y, Chen S D, Li W T. In: Niu Y J ed., Memoir of the 8th Annual Conf Transactions of Nonferrous Metals Society of China, Changsha: Central South University Press, 2010: 146

(潘颢丹, 杨洪英, 陈世栋, 李伟涛. 见: 钮因健 主编, 第八届中国有色金属年会会议论文集, 长沙: 中南大学出版社, 2010: 146)

[26] Fu B, Li H C eds.. Manual of Nonferrous Metallurgical Analysis. Beijing: Metallurgical Industry Press, 2004: 1

(符斌, 李华昌编. 有色冶金分析手册. 北京: 冶金工业出版社, 2004: 1)

[27] Yang H Y, Yang L, Wei X J. Trans Nonferrous Met Soc China, 2001; 11: 323

(杨洪英, 杨 立, 魏绪钧. 中国有色金属学报, 2001; 11: 323)

[28] Gebhardt J E, McCarron J J, Richardson P E, Buckley A N. Hydrometallurgy, 1986; 17: 27

[29] Harmer S L, Thomas J E, Fornasiero D, Gerson A R. Geochim Cosmochim Acta, 2006; 70: 4392

[30] Dora N, Ignacio G. Electrochim Acta, 2006; 51: 5295

[31] Weisener C G, Smart R St C, Gerson A R. Geochim Cosmochim Acta, 2003; 67: 823

[32] Yuri L M, Yevgeny V T, Igor P A, Alexander V O, Vladimir A V, Denis V V. Appl Surf Sci, 2005; 225: 395

[33] McIntyre N S, Zetaruk D G. Anal Chem, 1997; 49: 1521

[34] Klauber C, Parker A, Bronswijk W V, Watling H. Int J Miner Process, 2001; 62: 65

[35] Lazaro I, Nicol M J. In: Young C, Alfantazi A M, Anderson C G eds., Hydrometallurgy. Warrendale, PA: TMS, 2003: 405

[36] Stott M B,Watling H R, Franzmann P D, Sutton D. Miner Eng, 2000; 13: 1117
Outlines

/

〈 〉