论文

STRENTHENING MECHANISM OF MODULATED STRUCTURE INITIATED BY SPINODAL DECOMPOSITION

  • XU Jie-Yao
Expand
  • School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240

Received date: 2010-05-13

  Revised date: 2010-06-23

  Online published: 2011-01-11

Abstract

Through reviewing of a limited number of literatures regarding strengthening mechanism of modulated structure initiated by spinodal decomposition, it is found that the yield strength of aged alloy is mainly dependent on stress field built by the composition different between two precipitate phases which can be characterized by difference between lattice parameter Δa and is independent on modulate wave length and volume fraction of precipitate phase. However, in the ageing courses, the changes in yield stress and Δa did not show a linear relationship. The present author considers that this may be attributed to the local destruction of periodicity of modulated structure, causing change in stress field during ageing and suggests a yield stress equation: σc=MBΔa/a, in which M denotes a sum factor including Taylor (or Schmidt) factor and elastic constants, B, a factor represent the response of local stress field changed the function of Δa/a, Δa, the difference between lattice parameters of two precipitate phases and a, the average lattice parameter. This equation and the B value need to be confirmed and estimated.

Cite this article

XU Jie-Yao . STRENTHENING MECHANISM OF MODULATED STRUCTURE INITIATED BY SPINODAL DECOMPOSITION[J]. Acta Metall Sin, 2011 , 47(1) : 1 -6 . DOI: 10.3724/SP.J.1037.2010.00231

References

[1] Xu Z Y. Trans Mater Heat Treat, 2010; 31(1): 3

(徐祖耀. 材料热处理学报, 2010; 31(1): 3)

[2] Cahn J W. Acta Metall, 1963; 11: 1275

[3] Kato M, Mori T, Schwarrtz L H. Acta Metall, 1980; 28: 285

[4] Ditchek B, Schwartz L H. Ann Rev Mater Sci, 1979; 9: 219

[5] Hillert M, Cohen M, Averbach B L. Acta Metall, 1961; 9: 536

[6] Dahlgren S D. Metall Trans, 1977; 8A: 347

[7] Bradley A J. Proc Phys Soc, 1940; 52: 80

[8] Hargreaves M E. Acta Crystallogr, 1951; 4: 301

[9] Dahlgren S D. PhD Thesis, UCRL Report No.16846, University of California, Berkeley, Calif., 1966

[10] Dahlgren S D. Metall Trans, 1976; 7A: 1661

[11] Butler E P, Thomas G. Acta Metall, 1970; 18: 347

[12] Livak R J, Thomas G. Acta Metall, 1971; 19: 497

[13] Mott N F, Nabarro F R N. Proc Phys Soc, 1940; 52: 86

[14] Hirsch P B, Kelly A. Philos Mag, 1965; 12: 881

[15] Dillamore J L, Smallman R E, Roberts W J. Philos Mag, 1964; 9: 517

[16] Carpenter R W. Acta Metall, 1967; 15: 1297

[17] Fleischer R L. Electron Microscopy and Strength of Crystals, Hoboken: Wiley, 1963: 980

[18] Miyazaki T, Yajima E, Suga H. Trans JIM, 1971; 12: 119

[19] Ditchek B. PhD Thesis, Northwestern University, Evanston, IL., USA, 1978

[20] Ditchek B, Schwartz L H. Proc 4th Int Conf Strength of Metals and Alloys, 1976; 3: 1319

[21] Hanai Y, Miyazaki T, Mori H. J Mater Sci, 1979; 14: 599
Outlines

/

〈 〉