INFLUENCE OF SECOND–PHASE PARTICLES CONTAINING Ti ON MICROSTRUCTURE AND PROPERTIES OF WELD–HEAT–AFFECTED–ZONE OF A MICROALLOY STEEL

  • YU Wei ,
  • HE Shen-Lai ,
  • YU Hua-Min ,
  • LI Shu-Rui
Expand
  • 1. School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
    2. Wuhan Iron and Steel (Group) Corp, Wuhan 430080

Received date: 2010-03-19

  Revised date: 2010-05-28

  Online published: 2010-08-10

Supported by

Supported by High Technology Research and Development Program of China (No.2008AA03Z501)

Abstract

The effects of Ti–containing second–phase particles on the microstructure and properties of simulated welding heat affected zone (WHAZ) in a microalloy steel have been systematically investigated. The results show that the Ti deoxidized steel has a better low temperature impact toughness of simulated WHAZ than the Al deoxidized steel even in a longer phase change cooling time (t8/5=120 s, correspond to a welding heat input of 100 kJ/cm). The role of Ti–containing second–phase particls on improving the proprties ofWHAZ is mainly manifested in the following two aspects. First, theris a large number of Nb–containing TiOx–MnS particles with the size about several hundreds nanometers and Ti oxide containing NbC particles with the size less than 50 nm dispersed in the Ti deoxidized steel, these two kinds of small second–phase particles restrain the growth of austenite grain and refine the microstructure of WHAZ. Second, TiOx–MnS composite particles with the size between 1 μm to 3 μm can induce the nucleation of intragranular acicular ferrite (IAF) which could divide the prior autenite grain and refine tmicrostructure effectiely. As a result of the above two effects, the low temperature toughness of HAZ in Ti deoidized steel is significantly improved compared with the Al deoxidized steel.

Cite this article

YU Wei , HE Shen-Lai , YU Hua-Min , LI Shu-Rui . INFLUENCE OF SECOND–PHASE PARTICLES CONTAINING Ti ON MICROSTRUCTURE AND PROPERTIES OF WELD–HEAT–AFFECTED–ZONE OF A MICROALLOY STEEL[J]. Acta Metall Sin, 2010 , 46(8) : 997 -1003 . DOI: 10.3724/SP.J.1037.2010.00135

References

[1]Sasaki M, Ohsasa K, Kudoh M, Matsuura K.Refinement of Austenite Grain in Carbon Steel by Addition of Titanium and Boron[J].ISIJ Int,2008,48:340. [2]Alogab K A, Matlock D K, Speer J G, Kleebe H J.The Effects of Heating Rate on Austenite Grain Growth in a Ti-modified SAE 8620 Steel with Controlled Niobium Additions[J].ISIJ Int,2007,47:1034. [3]Lee J L, Pan Y T.Microstructure and toughness of the simulated heat-affected zone in Ti- and Al-killed steels[J].Materials Science & Engineering A,1991,A136:109. [4]Sarma D S, Karasev A V, Jonsson P G.On the role of non-metallic inclusions in the nucleation of acicular ferrite in steels[J].ISIJ Int,2009,49:1063. [5]Homma H, Ohkita S, Matsuda S, et al.IMPROVEMENT OF HAZ TOUGHNESS IN HSLA STEEL BY INTRODUCING FINELY DISPERSED Ti-OXIDE[J].Welding Journal ,1987,66:301. [6]Vega M I, Medina S F, Quispe A, et al.Influence of TiN particle precipitation state on static recrystallisation in structural steels[J].ISIJ Int, 2005,45:1878 [7]Ma Z T, Janke D. Oxide metallurgy - its purposes and practical approaches[J].Acta Metallurgica Sinica,1998,11:79 [8]Pan Y T, Lee J L.Development of TiOx-bearing steels with superior heat-affected zone toughness[J].Materials & Design,1994,15:331 [9]Hong S G, Kang K J, Park C G. Strain-induced precipitation of NbC in Nb and Nb-Ti microalloyed HSLA steels[J].Scripta Materialia, 2002,46:163 [10]Miodownik M A. Grain boundary engineering with particles[J].Scripta Materialia, 2006; 54:993 [11]Ricks R A, Howell P R, Barritte G S. The nature of acicular ferrite in HSLA steel weld metals[J].Journal of Materials Science, 1982; 17:732 [12]Barbaro F J, Krauklis P, Easterling K E.Formation of acicular ferrite at oxide particles in steels. Materials Science and Technology,1989,5:1057 [13]Lee Tae-Kyu, Kim H J, Kang B Y and Hwang S K. Effect of inclusion size on the nucleation of acicular ferrite in welds.ISIJ Int, 2000; 40:1260 [14]Al Hajeri, Khaled F. Particle-stimulated nucleation of ferrite in heavy steel sections. ISIJ Int, 2006; 46:1233 [15]Jye-Long Lee. Evaluation of the nucleation potential of intragranular acicular ferrite in steel weldments. Acta Metallurgica et Materialia, 1994; 42:3291 [16]Wu K M. Three-dimensional analysis of acicular ferrite in a low-carbon steel containing titanium.Scripta Materialia, 2006; 54:569 [17]Enomoto M, Wu K M, Inagawa Y, Murakami T, Nanba S. Three-dimensional observation of ferrite plate in low carbon steel weld.ISIJ Int, 2005; 45:756